Studies on the industrial application of "SHIRASU" (Report 8) : on the preparation of lightweight tile using "SHIRASU"
Bibliographic Information
- Other Title
-
- シラスの工業的利用に関する研究 (第8報) : シラスを原料とする白色タイル素地
- シラスの工業的利用に関する研究-8-シラスを原料とする白色タイル素地
- シラス ノ コウギョウテキ リヨウ ニ カンスル ケンキュウ 8 シラス オ ゲンリョウ ト スル ハクショク タイル キジ
Search this article
Description
A little amount of white cement, kaolin and wollastnite is added to magnetic separated and selected SHIRASU, the mixture then press moulded and fired in the electric furnace. Physical and thermal Properties and bending strength of those fired bodies were investigated. The properties of SHIRASU-white cement-kaolin system or SHIRASU-white cement-wollastnite system fired at 1150 to 1200°C are as follows, apparent gravity 2.3~2.7, bulk gravity 1.8~2.0, water absorption 0~17(%), bending strength 80~500kg/cm^2, and thermal expansion coefficient is found in the following region "5.6~5.8×10^{-6}". The whiteness of the tile bodies SHIRASU is 90(%), near the pure white, so that colouring is good and can be expected the reduction of pigment consumption.
Journal
-
- The research reports of the Faculty of Engineering, Kagoshima University
-
The research reports of the Faculty of Engineering, Kagoshima University 11 7-16, 1969-09
鹿児島大学
- Tweet
Details 詳細情報について
-
- CRID
- 1050282813855924352
-
- NII Article ID
- 120003055911
-
- NII Book ID
- AN00040363
-
- HANDLE
- 10232/11158
-
- NDL BIB ID
- 8143522
-
- ISSN
- 0451212X
-
- Text Lang
- ja
-
- Article Type
- departmental bulletin paper
-
- Data Source
-
- IRDB
- NDL
- CiNii Articles