Structural evolution at the oxidative and reductive limits in the first electrochemical cycle of Li1.2Ni0.13Mn0.54Co0.13O2

書誌事項

公開日
2020-03-06
権利情報
  • https://creativecommons.org/licenses/by/4.0
  • https://creativecommons.org/licenses/by/4.0
DOI
  • 10.1038/s41467-020-14927-4
公開者
Springer Science and Business Media LLC

説明

<jats:title>Abstract</jats:title><jats:p>High-energy-density lithium-rich materials are of significant interest for advanced lithium-ion batteries, provided that several roadblocks, such as voltage fade and poor energy efficiency are removed. However, this remains challenging as their functioning mechanisms during first cycle are not fully understood. Here we enlarge the cycling potential window for Li<jats:sub>1.2</jats:sub>Ni<jats:sub>0.13</jats:sub>Mn<jats:sub>0.54</jats:sub>Co<jats:sub>0.13</jats:sub>O<jats:sub>2</jats:sub> electrode, identifying novel structural evolution mechanism involving a structurally-densified single-phase A’ formed under harsh oxidizing conditions throughout the crystallites and not only at the surface, in contrast to previous beliefs. We also recover a majority of first-cycle capacity loss by applying a constant-voltage step on discharge. Using highly reducing conditions we obtain additional capacity via a new low-potential P” phase, which is involved into triggering oxygen redox on charge. Altogether, these results provide deeper insights into the structural-composition evolution of Li<jats:sub>1.2</jats:sub>Ni<jats:sub>0.13</jats:sub>Mn<jats:sub>0.54</jats:sub>Co<jats:sub>0.13</jats:sub>O<jats:sub>2</jats:sub> and will help to find measures to cure voltage fade and improve energy efficiency in this class of material.</jats:p>

収録刊行物

被引用文献 (2)*注記

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ