Selective growth of chirality-enriched semiconducting carbon nanotubes by using bimetallic catalysts from salt precursors
-
- Xiulan Zhao
- Beijing National Laboratory for Molecular Science
-
- Feng Yang
- Beijing National Laboratory for Molecular Science
-
- Junhan Chen
- Beijing National Laboratory for Molecular Science
-
- Li Ding
- Beijing National Laboratory for Molecular Science
-
- Xiyan Liu
- Beijing National Laboratory for Molecular Science
-
- Fengrui Yao
- State Key Laboratory for Mesoscopic Physics
-
- Meihui Li
- Beijing National Laboratory for Molecular Science
-
- Daqi Zhang
- Beijing National Laboratory for Molecular Science
-
- Zeyao Zhang
- Beijing National Laboratory for Molecular Science
-
- Xu Liu
- Beijing National Laboratory for Molecular Science
-
- Juan Yang
- Beijing National Laboratory for Molecular Science
-
- Kaihui Liu
- State Key Laboratory for Mesoscopic Physics
-
- Yan Li
- Beijing National Laboratory for Molecular Science
説明
<p>The controllable growth of 96% semiconducting SWNTs including 62% (14, 4) tubes was realized by using W–Co bimetallic catalysts.</p>
収録刊行物
-
- Nanoscale
-
Nanoscale 10 (15), 6922-6927, 2018
Royal Society of Chemistry (RSC)