Constitutional liquation during dissimilar friction stir welding of Al and Mg alloys
説明
Abstract A dissimilar friction stir weld of Al alloy 1050 and Mg alloy AZ31 was produced. The weld had a large volume of intermetallic compound Al 12 Mg 17 and significantly higher hardness in the weld center. The present study suggests that constitutional liquation resulted in the intermetallic compound Al 12 Mg 17 in the weld center.
収録刊行物
-
- Scripta Materialia
-
Scripta Materialia 50 (9), 1233-1236, 2004-05
Elsevier BV
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1361418518732041344
-
- NII論文ID
- 80016575083
-
- ISSN
- 13596462
-
- データソース種別
-
- Crossref
- CiNii Articles
- OpenAIRE