Fluoride release from a glass ionomer cement

書誌事項

公開日
1977-11
権利情報
  • http://onlinelibrary.wiley.com/termsAndConditions#vor
DOI
  • 10.1111/j.1600-0722.1977.tb00586.x
公開者
Wiley

この論文をさがす

説明

<jats:p><jats:bold><jats:sc>abstract</jats:sc> – </jats:bold> The release of fluoride from a glass ionomer cement (ASPA®) was. compared with that from a silicate cement. Test specimens were shaken in a solution with hydroxyapadte for 7 weeks. The solution was changed every week and the fluoride taken up by the hydroxyapatite measured. The specimens released considerably more fluoride during each of the first 2 weeks than during each of the subsequent 5 weeks. The continued release did not decrease very much with time. Slightly more fluoride was released from the glass ionomer cement than from the silicate.</jats:p>