Deuterium Retention of Carbon Dust. (II). Effect of Crystal Structure and Form.

Bibliographic Information

Other Title
  • カーボンダストの重水素保持特性 (II)  結晶構造と形状の影響
  • カーボンダスト ノ ジュウスイソ ホジ トクセイ 2 ケッショウ コウゾウ ト ケイジョウ ノ エイキョウ
  • Effect of Crystal Structure and Form
  • 結晶構造と形状の影響

Search this article

Abstract

Deuterium retention of carbon dust was investigated by two methods, i.e. one is deuterium gas absorption and the other is deuterium ion irradiation. After the gas absorption, retained deuterium desorbed in forms of D2 and HD. Saturated amount of retained deuterium due to the gas absorption at 100 Pa was approximately 10-3 in the atomic ratio D/C, when the temperature range was from 973 K to 1173 K. This amount was 10 or 100 larger than that of powdered graphite or bulk graphite, respectively. However, trapping energy of deuterium in the carbon dust was 0.22 eV, almost the same as that of the graphite. After the deuterium ion irradiation to the carbon dust, the retained deuterium desorbed in forms of D2, HD, CD4 and C2D4. The amount of retained deuterium due to the deuterium ion irradiation was 0.55 in the atomic ratio D/C, almost same as the graphite.

Journal

  • Shinku

    Shinku 44 (3), 310-313, 2001

    The Vacuum Society of Japan

References(8)*help

See more

Details 詳細情報について

Report a problem

Back to top