Description
This paper reports on the infrared study of the rehydrogenation of deuterated cellulose I and cellulose II with alcohols and water.<br>Deuteration of the crystalline region of cellulose II at room temperature was carried out. It was observed that all the hydroxyl groups in the crystalline region were completely deuterated. In the amorphous region, the rehydrogenation behaviour of the deuterated cellulose II with alcohols at room temperature is quite different from that with water, but in the crystalline region the difference is very slight.<br>It was shown, however, that the rehydrogenations of the resistant OD in the cellulose I and cellulose II with alcohols at temperatures from 110° to 170°C were not different from that with water.<br>It is most provable that the rehydrogenation of crystalline cellulose proceeded by proton transfer.
Journal
-
- Sen'i Gakkaishi
-
Sen'i Gakkaishi 28 (10), 381-386, 1972
The Society of Fiber Science and Technology, Japan
- Tweet
Keywords
Details 詳細情報について
-
- CRID
- 1390001204864252928
-
- NII Article ID
- 130004202429
-
- NII Book ID
- AN00131651
-
- ISSN
- 18842259
- 00379875
-
- NDL BIB ID
- 7569467
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed