チタン処理鋼中のチタンの態別定量

書誌事項

タイトル別名
  • Metallographic Analysis of Titanium in Titanium Treated Steel
  • チタン ショリ コウ チュウ ノ チタン ノ タイ ベツ テイリョウ

この論文をさがす

説明

A simple accurate method for the metallographic analysis of titanium in titanium treated steel is devised. The procedure is as follows:<BR>1. Separation of titanium:<BR>(a) Dissolve 1 g of sample in 30 ml of HCl (1: 2). Filter and wash with hot HCl (1: 9).<BR>(b) Dilute the filtrate to 50 ml in a volumetric flask, and determine titanium as solid solution continue in accordance with section 2 (a) to (c).<BR>(c) Transfer the paper and residue (Paragraph (a)) to the beaker, add 30 ml of HNO3 (1: 1) and boil for 5 min. Filter and wash with hot water.<BR>(d) Add 2 ml of H2SO4 to the filtrate and evaporate to a sirup. Dissolve salt with 40 ml of HC1 (1: 1), cool, dilute to 100 ml or 200 ml in a volumetric flask, and determine titanium as carbide continue in acordance with section 2 (a) to (c).<BR>(e) Transfer the paper and residue (Paragaph (c)) to the beaker, add 20 ml of HNO3 (1: 1) and 5 ml of H202, and boil for 10 min. Filter and wash with hot water.<BR>(f) Add 2 ml of H2SO4 to the filtrate and evaporate to a sirup. Disslove salt with 10 ml of HCl (1: 1), cool, dilute to 50 ml in a volumetric flask, and determine titanium as nitride continue in accordance with section 2 (a) to (c).<BR>(g) Transfer the paper and residue (Paragraph (e)) to the beaker, add 40 ml of HNO3, 3 ml of HClO4, and 2 ml of H2SO4, and evaporate to a sirup. Dissolve salt with 10 ml of HCl (1: 1), cool, dilute to 50 ml in a volumetric frask, and determine titanium as oxide continue in accordance with section 2 (a) to (c).<BR>2. Photometric determination of titanium:<BR>(a) Sample solution-Transfer 10 ml aliquot of solution Section (b), (d), (f) and (g) to 50 ml volumetric flask, add 5 ml of H2O and 8 ml of ascorbic acid solution (10%) to reduce iron, and then add 5 ml of HCl (1: 1) and 20 ml of diantipyrylmethane solution (1.5%), dilute to the mark.<BR>(b) Reference solution-Carry through all the steps of the procedure as directed in paragraph (a). However, no add diantipyrylmethane solution.<BR>(c) After 20 min, measure the absorbance against reference solution at 385 μ

収録刊行物

  • 鉄と鋼

    鉄と鋼 55 (4), 287-297, 1969

    一般社団法人 日本鉄鋼協会

被引用文献 (3)*注記

もっと見る

参考文献 (5)*注記

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ