Desiliconization, Desulfurization and [Mn] Increase of Hot Metal with CaO-MnO-CaF<SUB>2</SUB> Flux
-
- HANAO Masahito
- Corporate Research & Development Laboratories, Sumitomo Metal Industries, Ltd.
-
- MATSUO Tohru
- Corporate Research & Development Laboratories, Sumitomo Metal Industries, Ltd.
Bibliographic Information
- Other Title
-
- CaO-MnO-CaF<SUB>2</SUB>系フラックスによる溶銑の同時脱珪脱硫および[Mn]上昇
- CaO-MnO-CaF2系フラックスによる溶銑の同時脱珪脱硫および[Mn]上昇
- CaO MnO CaF2ケイ フラックス ニヨル ヨウセン ノ ドウジ ダツケ
Search this article
Description
Experiments were conducted on the hot metal treatment by adding CaO-MnO-CaF2 flux to 2kg carbon-saturated iron at 1350°C.<BR>(1) By adding CaO-MnO-CaF2 flux, desiliconization, desulfurization and [Mn] increase of carbon-saturated iron occurred simultaneously.<BR>(2) From the equilibrium oxygen partial pressure determined by [Si]-(SiO2) and that by [Mn] (MnO), the reaction: [Si]+2 (MnO)=2[Mn]+(SiO2) is considered to have almost reached equilibrium state.<BR>(3) By comparing Ls (=(%S)/[%S]) observed and that calculated using the numerical values of the sulfide capacity of CaO-SiO2-CaF2 slag and the equilibrium oxygen partial pressure, desulfurization is also considered to be in equilibrium state.
Journal
-
- Tetsu-to-Hagane
-
Tetsu-to-Hagane 83 (12), 779-784, 1997
The Iron and Steel Institute of Japan
- Tweet
Details 詳細情報について
-
- CRID
- 1390001205184352256
-
- NII Article ID
- 10003280138
-
- NII Book ID
- AN00151251
-
- ISSN
- 18832954
- 00211575
-
- NDL BIB ID
- 4344316
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed