CaSO?S4?T・2H?S2?TO,Ca(OH)?S2?T溶液における12CaO・7Al?S2?TO?S3?T組成のガラスの水和特性

書誌事項

タイトル別名
  • The Hydration Behaviors of Glassy 12CaO⋅7Al<sub>2</sub>O<sub>3</sub> in the Solution of CaSO<sub>4</sub>⋅2H<sub>2</sub>O or Ca(OH)<sub>2</sub>
  • CaSO4 2H2O Ca OH 2 ヨウエキ ニ オケル 12CaO 7Al

この論文をさがす

抄録

The authors investigated the hydration behaviors of glassy 12CaO⋅7Al2O3 containing SiO2 (3wt%) in the solution of CaSO4⋅2H2O or Ca(OH)2. The results were summarized as follows:<br>(1) Glassy 12CaO⋅7Al2O3 hydrated more slowly than crystalline 12CaO⋅7Al2O3.<br>(2) The eluted quantities of CaO or Al2O3 from glassy 12CaO⋅7Al2O3-H2O system were lower than crystalline 12CaO⋅7Al2O3, and they were CaO 0.6g/l, Al2O3 2.2g/l at long time.<br>(3) Ettringite formed at the first period of the hydration in the saturated solution or the suspension of CaSO4⋅2H2O. And 3CaO⋅Al2O3⋅6H2O formed in the saturated solution or the suspension of Ca(OH)2, while C2AH8 formed from crystalline 12CaO⋅7Al2O3.

収録刊行物

  • 窯業協會誌

    窯業協會誌 87 (1008), 400-404, 1979

    公益社団法人 日本セラミックス協会

被引用文献 (4)*注記

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ