Friction and Adhesion in Dry Warm Forging of Magnesium Alloy with Coated Tools

Abstract

In order to develop forging process of magnesium alloys without lubrication, frictional behavior of magnesium alloy AZ31B (Mg-3%Al-1%Zn) is evaluated by a tapered plug penetration test under dry condition. The cemented tungsten carbide (WC) plugs polished to be a mirror-like surface are coated with diamond-like carbon (DLC) and TiAlN by physical vapor deposition (PVD). The cylindrical hollow billets of AZ31B are penetrated by the tapered plugs at a temperature of 200°C. The surface roughness of the hole of the billet, the adhesion length of AZ31B on the plug surface and the penetration load are measured. Compared with WC and TiAlN coating, it is found that DLC coating is effective in preventing AZ31B from adhering to the tool surface and reducing the penetration load.

Journal

Citations (2)*help

See more

References(3)*help

See more

Related Articles

See more

Related Data

See more

Related Books

See more

Related Dissertations

See more

Related Projects

See more

Related Products

See more

Details

Report a problem

Back to top