The dependence of the conductivity of the Li(FexAl1-x)5O8 solid solution on its composition was investigated. The abrupt increase in the conductivity and decrease in the activation energy were observed between x=0.4 and 0.5 of Li(FexAl1-x)5O8. The composition x=0.415, which corresponds to the percolation threshold expected from the percolation theory, is within this range (x=0.4-0.5). The conductivities of the compositions above the percolation threshold were revealed to increase as (p-pSC)2.0(pSC=0.311). Consequently, the abrupt increase in the conductivity is attributed to the formation of the conducting or percolation path of Fe ions among the B-sites of the spinel.
収録刊行物
-
- Journal of the Ceramic Society of Japan (日本セラミックス協会学術論文誌)
-
Journal of the Ceramic Society of Japan (日本セラミックス協会学術論文誌) 105 (1221), 446-448, 1997
公益社団法人 日本セラミックス協会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390001205278527232
-
- NII論文ID
- 110002289184
-
- NII書誌ID
- AN10040326
-
- ISSN
- 18821022
- 09145400
-
- NDL書誌ID
- 4205703
-
- データソース種別
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可