Relationship between Pitting of Aluminum Alloy 5052 and Concentration of Dissolved Oxygen for Can Stocks
-
- Seri Osami
- Muroran Institute of Technology
-
- Furuya Shyuichi
- Technical Research Lab., Furukawa Aluminum Co., Ltd.
-
- Soga Noboru
- Technical Research Lab., Furukawa Aluminum Co., Ltd.
Bibliographic Information
- Other Title
-
- 缶用アルミニウム合金5052の孔食と缶内溶存酸素の関係
- カンヨウ アルミニウム ゴウキン 5052 ノ コウショク ト カンナイ ヨウ
Search this article
Abstract
The area polarization method was applied to the corrosion monitoring of aluminum alloy 5052, which was galvanically coupled with tinplate. This was measured by changing the disolved oxygen <1-6, 000ppb in the 1, 000ppm NaCl solution. It was concluded that the possibility of pitting corrosion of the aluminum alloy 5052 becomes higher, under the condition of over 30-60ppb dissolved oxygen in the 1, 000ppm NaCl solution.
Journal
-
- CORROSION ENGINEERING
-
CORROSION ENGINEERING 39 (4), 175-178, 1990
Japan Society of Corrosion Engineering
- Tweet
Details 詳細情報について
-
- CRID
- 1390001206257634688
-
- NII Article ID
- 130006025311
- 130004732166
-
- NII Book ID
- AN00225595
-
- ISSN
- 18841155
- 00109355
-
- NDL BIB ID
- 3668829
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed