- Kohiki Shigemi
- Department of Materials Science, Kyushu Institute of Technology
-
- Hori Kyoko
- Department of Materials Science, Kyushu Institute of Technology
-
- Kawaguchi Akinori
- Department of Materials Science, Kyushu Institute of Technology
-
- Murakawa Yusuke
- Department of Materials Science, Kyushu Institute of Technology
-
- Shimooka Hirokazu
- Department of Materials Science, Kyushu Institute of Technology
-
- Tajiri Takayuki
- Department of Electronic Engineering, Kyushu Institute of Technology
-
- Deguchi Hiroyuki
- Department of Electronic Engineering, Kyushu Institute of Technology
-
- Mitome Masanori
- National Institute of Materials Science
-
- Bando Yoshio
- National Institute of Materials Science
-
- Fukushima Sei
- National Institute of Materials Science
-
- Arai Masao
- National Institute of Materials Science
-
- Oku Masaoki
- Institute for Materials Research, Tohoku University
-
- Shishido Toetsu
- Institute for Materials Research, Tohoku University
書誌事項
- タイトル別名
-
- Dilution Effects on Chemical and Magnetic Clusters of .ALPHA.-LiFeO2
- Dilution Effects on Chemical and Magnetic Clusters of アルファ LiFeO2
- Dilution Effects on Chemical and Magnetic Clusters of α-LiFeO<sub>2</sub>
この論文をさがす
抄録
We have synthesized α-LiFe1−xInxO2 (x=0, 0.001, 0.01, 0.05, and 0.1) powders by calcination of Li2CO3, Fe2O3 and In2O3 mixtures. In X-ray diffraction, the sample with larger x value showed larger lattice constant of the cubic NaCl-type structure. Aside from electron diffraction patterns of the cubic unit cell with diffuse scattering for both the samples, the x=0 sample demonstrated a doubled structure of the cubic unit cell with wavy diffuse scattering, though the x=0.1 sample exhibited the doubled structure with less intensive diffuse scattering. In cooling history-dependent dc susceptibilities, the bifurcation point of the x=0 sample was ≈90 K, and it lowered from 87 to 44 K with increasing the x value from 0.001 to 0.1. Dilution of α-LiFeO2 with nonmagnetic In3+ ions suppressed chemical cluster formation at room temperature and reduced temperature of ferromagnetic cluster formation.
収録刊行物
-
- Japanese Journal of Applied Physics
-
Japanese Journal of Applied Physics 43 (12B), L1620-L1622, 2004
The Japan Society of Applied Physics
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390001206265427840
-
- NII論文ID
- 10015473798
- 210000057107
-
- NII書誌ID
- AA11906093
-
- ISSN
- 13474065
- 00214922
-
- NDL書誌ID
- 7193835
-
- 本文言語コード
- en
-
- データソース種別
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可