- 田中 一郎
- 九州歯科大学第2補綴学教室:九州歯科大学歯科理工学教室
書誌事項
- タイトル別名
-
- A Stuby on Strain-Aging of Dental Cobalt-Chromium Alloy Wires : Rep. 1 The Effects on the Mechanical Properties by Low-Temperature Annealing
- 歯科用コバルト・クロム合金線のひずみ時効に関する研究-1-低温焼なましによる機械的性質の変化
- シカヨウ コバルト クロム ゴウキンセン ノ ヒズミ ジコウ ニ カンスル ケンキュウ 1 テイオン ヤキナマシ ニ ヨル キカイテキ セイシツ ノ ヘンカ
この論文をさがす
説明
On the present paper, preliminary experiments on the effects of cold-working upon the strainaging of Co-Cr alloy wires were performed. Each wire has the same constitution but different diameter. The author, in fact, estimated the effects of the amount of cold-working upon their mechanical properties at various temperatures of annealing for one hour. Results obtained were as follows : 1. It was found that the peak of hardening appeared by annealing at about 500℃. 2. The larger was the amount of cold-working, the more increased the aging effect. 3. Consepuently, this treatment may be recommended for the prosthetic application of the fine wires.
収録刊行物
-
- 九州歯科学会雑誌
-
九州歯科学会雑誌 21 (4), 393-396, 1968
九州歯科学会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390001206348719232
-
- NII論文ID
- 110003008195
-
- NII書誌ID
- AN00054335
-
- ISSN
- 18808719
- 03686833
-
- NDL書誌ID
- 8160990
-
- 本文言語コード
- ja
-
- データソース種別
-
- JaLC
- NDLサーチ
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可