抄録
In order to investigate the effects of non-metallic inclusions on the strength of steels, the behavior of non-metallic inclusions under tensile stress was studied by microscopic observations and the fatigue properties of several 3%Ni-Mo-V steels made by different processes were tested. The results were as follows: (i) At a slight excess load over the yielding point, microcracks are found at the corners of non-metallic inclusions, especially on the transverse specimen; (ii) between the elongated type inclusions, silicate is more harmful than sulfide to transverse fatigue properties; and this is borne out by the higher strain concentration evident at the silicate during tensile test; (iii) the effect of sulfide on fatigue properties does not exceed 10%, even though the sulfide content is rather high and vacuum-poured electric-arc furnace steel has good cleanliness and good fatigue properties; and (iv) the notched fatigue strength shows little anisotropy.
収録刊行物
-
- 日本金属学会誌
-
日本金属学会誌 25 (8), 510-515, 1961
公益社団法人 日本金属学会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390001206481189504
-
- NII論文ID
- 130007332589
- 40018257979
-
- NII書誌ID
- AN00187860
-
- ISSN
- 18806880
- 24337501
- 00214876
-
- NDL書誌ID
- 9153419
-
- データソース種別
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可