鉄塩の分解および酸化鉄粉の加熱による比表面積変化

書誌事項

タイトル別名
  • The Changes in Specific Surface Area of Iron Salts and Iron Oxides Powders by Heating
  • テツエン ノ ブンカイ オヨビ サンカ テップン ノ カネツ ニ ヨル ヒ ヒョウメンセキ ヘンカ

この論文をさがす

抄録

The surface behaviors of the iron oxides in loose powder mass were studied. The results from the following three experiments are described: (i) Measurement of the specific surface area of iron oxides produced by the thermal decomposition of iron salts, (ii) the changes of the specific surface area of iron oxide powder by heating at constant temperatures, (iii) the densification of iron oxides. All the experiments were conducted under atmospheric pressure. By heating Fe (III) salts, the surface area of oxides suffered regular changes, but in the case of Fe (II) salts, random changes of the surface area were observed. The rate of contraction of the surface area of iron oxides by heating can be described by the next formula; −dVtdt=kVt, and its activation energy is about 10 kcal/gmole.

収録刊行物

  • 日本金属学会誌

    日本金属学会誌 24 (11), 699-703, 1960

    公益社団法人 日本金属学会

詳細情報 詳細情報について

問題の指摘

ページトップへ