Abstract
An attempt was made to identify oxides on 0∼2.5 wt%Be-elinvars at 800°C and 1100°C in a dissociated-ammonia gas and in air. For this, electron and X-ray diffraction methods were adopted. An X-ray microanalyser and an optical microscope were employed complementally in the observation of the oxides. The results obtained are as follows;<BR>(1) BeO was formed selectively on the surfaces of 0.5∼2.5 wt%Be-elinvars heated in a dissociated-ammonia gas at 800°C and 1100°C for a few minutes.<BR>(2) On the surfaces of 1.2∼2.5 wt%Be-elinvars heated in air at 1100°C for 1 hour, BeO was formed predominantly.<BR>(3) The surfaces of 0∼1.2 wt%Be-elinvars exposed in air at 1100°C for 1 hour were covered with layer oxides—α-Fe2O3 (outer layer), spinel type oxide or (Fe, Ni, Cr)3O4 (inner layer).<BR>(4) A thin BeCr2O4 film, in the same condition as above, spread itself on the surface of 2.5 wt%Be-elinvar, in pores of which the patches of oxides with layer structures were dispersed.
Journal
-
- Journal of the Japan Institute of Metals and Materials
-
Journal of the Japan Institute of Metals and Materials 31 (2), 109-113, 1967
The Japan Institute of Metals and Materials
- Tweet
Details 詳細情報について
-
- CRID
- 1390001206481695488
-
- NII Article ID
- 130007333313
- 40018256126
-
- NII Book ID
- AN00187860
-
- ISSN
- 18806880
- 24337501
- 00214876
-
- NDL BIB ID
- 8371440
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed