Post-breakaway Oxidation of Zirconium and its Alloys
Bibliographic Information
- Other Title
-
- ジルコニウムおよびその合金の後期酸化
- ジルコニウム オヨビ ソノ ゴウキン ノ コウキ サンカ
Search this article
Abstract
The post-breakaway oxidation rate of reactor grade pure zirconium, 2.5% tin-zirconium and 0.24% iron-zirconium alloy in dry oxygen and air were measured over the temperature range of 500∼850°C and pressure range of 15∼760 mmHg. The results were as follows: (1) A lower oxidation rate and its pressure dependence were found in the oxidation of pure zirconium and 0.24% iron-zirconium alloy in oxygen. (2) A higher oxidation rate and its pressure dependence were found in the oxidation of 2.5% tin-zirconium alloy in oxygen and air. (3) In the case of air oxidation of pure zirconium and 0.24% iron-zirconium alloy the oxidation rate and its pressure dependence increased remarkably with temperature. (4) Thus, a correspondence between oxidation rate and its pressure dependence were found.
Journal
-
- Journal of the Japan Institute of Metals and Materials
-
Journal of the Japan Institute of Metals and Materials 23 (7), 385-388, 1959
The Japan Institute of Metals and Materials
- Tweet
Details 詳細情報について
-
- CRID
- 1390001206481878912
-
- NII Article ID
- 130007333553
- 40018257466
-
- NII Book ID
- AN00187860
-
- ISSN
- 18806880
- 24337501
- 00214876
-
- NDL BIB ID
- 9152906
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed