Thin wires of α brass and aluminium were elongated at various temperatures and quenched in water immediately after working. The micro-hardness of these wires were measured at room temperature and a remarkable work hardening was found even on the specimens elongated at the so-called hot-working temperature range. The work hardenings at various temperatures became larger with increasing working degrees. The load-elongation curves at high temperatures were recorded and were discussed in comparison with work hardenings of the same specimens measured at room temperature.