To evaluate the groove cracking resistance of the tire tread compound in the laboratory, A. S. T. M. D-813 or its modified methods, in general, have been employed.<br>But it is said that the laboratory test results are poorly reproducible and rarely agree with practical experience.<br>In order to improve the correlation between the laboratory data and the actual road test results, we carried out the experiment, using the modified W. Kern method.<br>By applying this new method to the tread compounds including N. R, SBR, Polybutadiene, and Cis 1.4 Polyisoprene respectively, we obtained laboratory results better reproducible and agreeable with road service performance than by A. S. T. M. method.<br>Next, the research for testing the effect of ozone, ambient temperature and flexing speed on the groove cracking resistance of variable polymer was carried out, using three typical method, i. e. crack initiation, cut growth, and crack formation (W. Kern′s) methods. Increase of flexing speed from 300r.p.m to 600r.p.m led to slight decrease of the rate of crack growth and formation.<br>Finally, the experiment for testing the effect of typical antioxidants and antiozonants in the natural rubber tread compounds with three method was carried out.

収録刊行物

  • 日本ゴム協会誌

    日本ゴム協会誌 35 (10), 738-745, 1962

    一般社団法人 日本ゴム協会

詳細情報 詳細情報について

問題の指摘

ページトップへ