This study was investigated in order to develop recovery system of phosphate and ferric chloride from precoagulated sludge with ferric chloride. Experiments were conducted to clear the following points, Dextraction efficiency of phosphate from pre-coagulated sludge with ferric chloride by introducing H2S gas into sludge, 2) recovery of phosphate from the supernatant after the extraction using Ca (OH) 2, 3) simultaneous recovery of ferric chloride and H2S from the residue after the extraction by adding HCl solution and 4) the mass balance of suspended solid, phosphorus, iron and sulfur in this total system. As the result of mass balance in this system, 40% of phosphate and 73.1% of ferric chloride from precoagulated sludge with ferric chloride and 47.2% of introduced H2S gas were recovered at the optimum experimental condition.

収録刊行物

詳細情報 詳細情報について

  • CRID
    1390282679088248576
  • NII論文ID
    130003949289
  • DOI
    10.11532/proes1992.38.323
  • ISSN
    1884829X
    13415115
  • 本文言語コード
    ja
  • データソース種別
    • JaLC
    • CiNii Articles
  • 抄録ライセンスフラグ
    使用不可

問題の指摘

ページトップへ