Effect of Preservation in the Air on the Hydriding Characteristics of the LaNi4.7Al0.3 Alloy Treated by Anhydrous Hydrogen Fluoride.
-
- ITO Manabu
- R & D Dept, Benkan Corp.
-
- AONO Fumiaki
- R & D Dept, Benkan Corp.
-
- KOSUGE Akiyoshi
- R & D Dept, Benkan Corp.
-
- HIRAYAMA Ryouji
- R & D Dept, Stella Chemifa Corp
-
- KIKUYAMA Hirohisa
- R & D Dept, Stella Chemifa Corp
-
- KAMASAKI Seiji
- Fac. of Eng, Tokyo Metropolitan Univ
Bibliographic Information
- Other Title
-
- 無水フッ化水素で表面改質したLaNi4.7Al0.3の水素吸蔵特性におよぼす大気保存の影響
- ムスイ フッカ スイソ デ ヒョウメン カイシツシタ LaNi4.7Al0.3
Search this article
Abstract
Hydriding characteristics of LaNi4.7Al0.3 alloys with surfaces modified by high-purity anhydrous HF were evaluated after long-term preservation in air. Affected by poisoning species in air, untreated alloy hydriding activity was enormously decreased. HF-treated alloys with a modified surface layer containing metal fluoride NiF2, LaF3 and AlF3 maintained relatively high activity. In high-humidity air, metal fluoride NiF2 reacted with moisture to form hydrous Ni(OH)2, and permeation of poisonous species such as O2, CO and CO2 was markedly inhibited by moisture-condensed hydrate screens.
Journal
-
- Journal of The Surface Finishing Society of Japan
-
Journal of The Surface Finishing Society of Japan 48 (12), 1207-1211, 1997
The Surface Finishing Society of Japan
- Tweet
Details 詳細情報について
-
- CRID
- 1390282679091938176
-
- NII Article ID
- 10002260594
-
- NII Book ID
- AN1005202X
-
- ISSN
- 18843409
- 09151869
-
- NDL BIB ID
- 4367243
-
- Text Lang
- ja
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed