Abstract
Antifouling paint on the shell bottom performs functions of making the surface of the shell bottom smooth and preventing an increase in frictional resistance by preventing the attachment of marine growth thereto. For three kinds of antifouling paints different in antifouling system, we have carried out a rotor test in sea water, and measured the surface roughness by using a surface roughness gauge and observed the paint film cross section by an electron scanning microscope. In regard to the leaching behaviour of antifouling agent and the change of paint film surface condition, the following results have been found : 1) The leaching rate of antifouling agent obtained in the rotor test in sea water is 70-150 times that in immersion test in still sea water. 2) To prolong the life of antifouling paint, it is effective to control the diffusion of antifouling agent in paint film. 3) In such conditions as in the rotor test in sea water, the surface roughness hardly changes. Thus, we have confirmed that this investigation is useful to clear the relation between the leaching behaviour of antifouling agent and the antifouling performance.
Journal
-
- Journal of the Kansai Society of Naval Architects, Japan
-
Journal of the Kansai Society of Naval Architects, Japan 174 (0), 9-15, 1979
The Japan Society of Naval Architects and Ocean Engineers
- Tweet
Details 詳細情報について
-
- CRID
- 1390282679473472384
-
- NII Article ID
- 110003873357
-
- NII Book ID
- AN00349587
-
- ISSN
- 2433104X
- 03899101
-
- NDL BIB ID
- 2062591
-
- Text Lang
- ja
-
- Data Source
-
- JaLC
- NDL
- CiNii Articles
-
- Abstract License Flag
- Disallowed