Effect of Adhesive Primer Developed Exclusively for Heat-curing Resin on Adhesive Strength between Plastic Artificial Tooth and Acrylic Denture Base Resin
-
- NISHIGAWA Goro
- Clinical Division of Removable Prosthodontics, Okayama University Hospital of Dentistry
-
- MARUO Yukinori
- Department of Occlusal and Oral Functional Rehabilitation, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
-
- OKAMOTO Makoto
- Department of Occlusal and Oral Functional Rehabilitation, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
-
- OKI Kazuhiro
- Department of Occlusal and Oral Functional Rehabilitation, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
-
- KINUTA Yoshihiro
- Department of Occlusal and Oral Functional Rehabilitation, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
-
- MINAGI Shogo
- Department of Occlusal and Oral Functional Rehabilitation, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
-
- IRIE Masao
- Department of Biomaterials, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
-
- SUZUKI Kazuomi
- Department of Biomaterials, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
この論文をさがす
抄録
Despite progress in the development of denture base resin and artificial tooth materials, dental clinics are still plagued with artificial teeth falling off the denture base - due to poor bond strength - after denture delivery. Against this background, this study sought to examine the effect and durability of an adhesive primer developed exclusively for heat-curing resin on the adhesive strength of heat-curing denture base acrylic resin to plastic artificial tooth. Test specimens were divided into four groups according to the treatment method of the artificial tooth's test bonding surface: air abrasion, adhesive primer application, adhesive primer application after air abrasion, and pretreatment only (control) . After heat curing of acrylic resin onto the bonding surface, shear test was performed for two storage periods: 24-hour versus 100-day water storage. From the results obtained, it was revealed that the evaluated adhesive primer was significantly effective in increasing adhesive strength between artificial tooth and acrylic resin, although specimens were stored in water for 100 days.
収録刊行物
-
- Dental Materials Journal
-
Dental Materials Journal 25 (1), 75-80, 2006
一般社団法人 日本歯科理工学会
- Tweet
詳細情報
-
- CRID
- 1390282679693854336
-
- NII論文ID
- 110004498259
-
- NII書誌ID
- AA10443149
-
- COI
- 1:CAS:528:DC%2BD28XltFamu7o%3D
-
- ISSN
- 18811361
- 02874547
-
- 本文言語コード
- en
-
- データソース種別
-
- JaLC
- Crossref
- NDL-Digital
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可