  • On the Formation of Asperity on Worn Surfaces (6th Report)
  • Experimental Investigations on the Results of Theoretical Analysis of Steady Wear (In the Case of Pyrex Glass)
  • 定常摩耗の解析に関する実験的検討 (パイレックスガラスの場合)

抄録

The experimental investigations are carried out with Pyrex glass in regard to the results of theoretical analysis of steady wear which are introduced in 5th report. The main results obtained are as follows : <BR>(1) In relatively low range of sliding velocity υ, wear volumes per unit time are nearly constant, but increase abruptly as υ is increased, in higher range of υ.<BR>(2) The wear rate Vl is minimized at critical sliding velocity υc and the relation between Vl and υc agrees qualitatively with the results of theoretical analysis in 5th report. Assuming the activation energy Δf to be 20 kcal/mol, calculated value of υc is relatively close to that obtained experimentally.<BR>(3) In this experiments, the ratio of the number of elastic contacts to the number of total contacts is analytically obtained to be I.

収録刊行物

  • 精密機械

    精密機械 43 (508), 403-408, 1977

    公益社団法人 精密工学会

詳細情報 詳細情報について

  • CRID
    1390282679742221056
  • NII論文ID
    130003961187
  • DOI
    10.2493/jjspe1933.43.403
  • ISSN
    03743543
  • データソース種別
    • JaLC
    • Crossref
    • CiNii Articles
  • 抄録ライセンスフラグ
    使用不可

問題の指摘

ページトップへ