高速対応型快削鋼のエンドミル加工: BN添加鋼切削時の工具摩耗と切削温度

書誌事項

タイトル別名
  • End Milling of Free-machining Steel for High Speed Machining
  • 高速対応型快削鋼のエンドミル加工
  • コウソク タイオウガタ カイサクコウ ノ エンドミル カコウ BN テンカ コウ セッサクジ ノ コウグ マモウ ト セッサク オンド
  • —Tool Wear and Cutting Temperature in Cutting BN Added Steels—
  • —BN添加鋼切削時の工具摩耗と切削温度—

この論文をさがす

抄録

This paper deals with the machinability of BN added Steels in end milling. The cutting tests were carried out by end milling carbon steel JIS S45C, S55C and these BN added steels with carbide tool and TiAlN coated carbide tool. Tool wear, cutting temperature, and, surface roughness were measured and discussed. In end milling BN added steel with square end mill, the progress rate of flank wear width was decreased and fracture at corner was suppressed in comparison with that in machining standard steel. In case of ball end mill, flank wear in end milling BN added steels were smaller in comparison with standard steel. In case of S45C, boundary wear was observed, however it was not observed in end milling BN added steel. BN added showed almost the same surface roughness as standard steel. The temperature of flank wear part in turning work based S55C were 50 °C higher in comparison with S45C base work. The temperature of throw away end mill was higher 100°C in comparison with solid square end mill. There were not significant difference between the temperature in end milling standard steel and BN added steels.

収録刊行物

  • 精密工学会誌

    精密工学会誌 73 (7), 803-807, 2007

    公益社団法人 精密工学会

被引用文献 (1)*注記

もっと見る

参考文献 (11)*注記

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ