This paper describes the influence of electrolytically oxidized water dilute NaCl on the surface of pure nickel. First, we clarified the etching characteristic of electrolytically-oxidized water of dilute NaCl against the surface of pure nickel using HCl solution for comparative immersion experiments. The results show electrolytically-oxidized water works well for the etching operation, and if the ORP/pH value of the electrolytically-oxidized water is high, the etching speed becomes correspondingly fast. The etching rate of electrolytically-oxidized water is high (about 3 times) compared with the HCl solution of the same pH value. Next, by the observation of the SEM image and surface roughness, the influence of electrolytically oxidized water on the shape of the pure nickel surface became clear. Lastly, auger analysis revealed that the natural-oxidation film of the pure nickel can be removed with electrolytically oxidized water. The study indicates that electrolytically oxidized water can be applied to the surface treatment and washing of pure nickel.
収録刊行物
-
- 精密工学会誌
-
精密工学会誌 76 (6), 633-637, 2010
公益社団法人 精密工学会
- Tweet
キーワード
詳細情報 詳細情報について
-
- CRID
- 1390282679773650304
-
- NII論文ID
- 130000421840
-
- NII書誌ID
- AN1003250X
-
- ISSN
- 1882675X
- 09120289
-
- NDL書誌ID
- 10733367
-
- データソース種別
-
- JaLC
- NDL
- Crossref
- CiNii Articles
- KAKEN
-
- 抄録ライセンスフラグ
- 使用不可