Some experiments on the rate of silica reduction by carbon saturated iron have been carried out in the range of 1550-1620°C and kinetics of silica reduction has been considered combining the present results with already published data by many investigators.<BR>The results obtained are as follows:<BR>1. The reduction of silica in a graphite crucible is promoted by the increase of slag-graphite interface area, Al addition to metal and application of external electric potential.<BR>2. Present result and the results already published by many investigators on the silica reduction have been put in order by considering the ratio γ=Ss-G/Ss-M-. In small value of γ, the rate of reaction is pro-portional to activity of silica in CaO-SiO2binary slag and apparent activation energy of silica reduction is about 90-100 kcal/mol. In this condition, silica reduction is controlled by chemical reaction in general but diffusion sometimes affect the rate according to the composition and transport properties such as viscosity of slag. On the contrary, in the range of γ>30 up to the present experiment diffusion step of silicate ion in slag is considered to be the limiting step.

収録刊行物

  • 鉄と鋼

    鉄と鋼 54 (14), 1437-1446, 1968

    一般社団法人 日本鉄鋼協会

被引用文献 (2)*注記

もっと見る

参考文献 (3)*注記

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ