書誌事項
- タイトル別名
-
- Synthesis of PbTe by Reduction of Corresponding Oxide with Metal Bis(trimethylsilyl)amide as Starting Chemicals
- キンゾク ビスアミド オ ゲンリョウ ケミカル ト スル サンカブツ カンゲンホウ ニ ヨル PbTe ノ ゴウセイ
この論文をさがす
説明
A new synthetic route based on solution chemistry was developed for a compound semiconductor lead telluride (PbTe). Lead telluride was synthesized by reduction of PbTeO3, which was prepared by hydrolysis of the corresponding metal organic solution as starting material. Two kinds of metal organic solution, metal bis(trimethylsilyl)amide and metal alkoxide were used as starting chemicals. PbTe-bisamide solution was prepared by the reaction of lead chloride with Li-bisamide in the presence of Te-bisamide. PbTe-alkoxide solution was prepared by the alcoholysis reaction of PbTe-bisamide with BuOH. Amorphous PbTeO3 was obtained by hydrolysis of the PbTe-bisamide and PbTe-alkoxide. Heat-treatment of the resulting amorphous PbTeO3 powder at 250°C and 400°C in air resulted in the transformation to a cubic PbTeO3 phase and to a tetragonal PbTeO3 phase, respectively. PbTe was obtained by heat-treatment of calcined amorphous and crystallized PbTeO3 at 400°C-500°C in H2. The Pb/Te ratios of the products were chemically stoichiometric.<br>
収録刊行物
-
- Journal of the Ceramic Society of Japan (日本セラミックス協会学術論文誌)
-
Journal of the Ceramic Society of Japan (日本セラミックス協会学術論文誌) 113 (1316), 286-290, 2005
公益社団法人 日本セラミックス協会
- Tweet
キーワード
詳細情報 詳細情報について
-
- CRID
- 1390282680225369984
-
- NII論文ID
- 110002292296
-
- NII書誌ID
- AN10040326
-
- ISSN
- 18821022
- 09145400
-
- NDL書誌ID
- 7301254
-
- 本文言語コード
- ja
-
- データソース種別
-
- JaLC
- NDL
- Crossref
- CiNii Articles
- KAKEN
- OpenAIRE
-
- 抄録ライセンスフラグ
- 使用不可