1573KにおけるFeOx- SiO<sub>2 </sub>系スラグの白金の溶解度

書誌事項

タイトル別名
  • The Solubility of Platinum in the FeOx-SiO<sub>2</sub> Slag at 1573K
  • 1573KにおけるFeOx-SiO₂系スラグの白金の溶解度
  • 1573K ニ オケル FeOx-SiO ₂ ケイ スラグ ノ ハッキン ノ ヨウカイド
  • The Solubility of Platinum in the FeOx-SiO2 Slag at 1573K

この論文をさがす

抄録

There is an increasing trend in the copper smelters to recycle electronic materials, which contain relatively high concentration of platinum group metals. Platinum group metals lost in the slag is increasing with increasing of treated scrap amount. To determine the portion of the platinum group metals chemically dissolved in the slag will be a key factor to improve the recovery of those metals. An experimental study was carried out to determine the solubility of platinum in FeOx-SiO2 slag equilibrated with a pure platinum and the liquid Pt-Cu alloy at 1573 K and the range of oxygen partial pressure from 10-9 to 10-6. The solubility of platinum in the slag tends to increase with increasing oxygen partial pressure and content of copper in the slag. Based on the measured platinum solubility, activity coefficients of platinum oxide in the FeOx-SiO2 slag were derived. The activity coefficients decrease by increasing copper contents in slag. Therefore, lower copper content in the slag tend to lower precious metals dissolution in the slag.

収録刊行物

  • 資源と素材

    資源と素材 129 (5), 208-212, 2013

    一般社団法人 資源・素材学会

被引用文献 (6)*注記

もっと見る

参考文献 (14)*注記

もっと見る

関連プロジェクト

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ