抄録

We previously reported on needle damage to needles sterilized 50 times. This time we increased the number of sterilizations to 100 times and investigated needle damage. damage.<br>Sterilization was performed using a small high pressure steam sterilizer at a temperature of 126°C for 25 minutes each time.<br>1. Non-gold or silver needles had a tendency to become finer but there was no remarkable weight change noted.<br>2. Resistance to bending tests showed that Chinese needles become more difficult to break.<br>3. Elasticity tests showed that non-gold needles become easier to restore to their original state.<br>4. Insertion tests showed that some needles, especially Chinese needles and stainless steel No. 3 needles, become more difficult to insert smoothly.<br>5. Hardness and sturdiness tests showed a general decrease in both factors with the exception of hard silver No. 3 needles and Chinese needles which become sturdier.

収録刊行物

詳細情報 詳細情報について

  • CRID
    1390282680375711872
  • NII論文ID
    130004386642
  • DOI
    10.11525/jjsam1955.30.105
  • ISSN
    21859434
    05461367
  • 本文言語コード
    ja
  • データソース種別
    • JaLC
    • CiNii Articles
  • 抄録ライセンスフラグ
    使用不可

問題の指摘

ページトップへ