- Effect of Specimen Configuration on Crack Initiation Behavior of Delayed Failure
- オクレ ハカイ キレツ ハッセイ キョドウ ニ オヨボス シケンヘン ケイジョ
- 見掛けの応力拡大係数による検討
この論文をさがす
抄録
The crack initiation behavior in delayed failure was studied on various specimen configurations, using the apparent stress intensity factor, Ka, which is obtained by substituting notch length for crack length in the equation of stress intensity factor K.<br>When Ka is constant, the time to crack initiation is independent of notch length a0 and loading methods, but is dependent on specimen thickness B and notch root radius ρ. When the crack initiation time is constant, the next experimental equation holds:<br>Ka=KI(B0/B)δ(ρ/ρ0)λ, ρ≥ρ0<br>where KI is the stress intensity factor under plane strain state, B0 is the critical specimen thickness over which crack initiation time is constant, ρ0 is the critical notch root radius under which Ka at crack initiation is constant, and δ and λ are constant. ρ0 varies with crack initiation time and seems to depend not only on mechanical factors but also on chemical factors, such as the formation of protective film on the notch root surface.
収録刊行物
-
- 材料
-
材料 28 (307), 299-305, 1979
公益社団法人 日本材料学会
- Tweet
キーワード
詳細情報 詳細情報について
-
- CRID
- 1390282680396285696
-
- NII論文ID
- 110002298104
-
- NII書誌ID
- AN00096175
-
- ISSN
- 18807488
- 05145163
-
- NDL書誌ID
- 2049110
-
- 本文言語コード
- ja
-
- データソース種別
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可