書誌事項
- タイトル別名
-
- 227 Peak separation of trapped hydrogen at various oalltice defects by thermal desorption spectrometry
説明
Hydrogen embrittlement has been analyzed by using thermal desorption spectrometry (TDS). However, it is difficult to separate the states of trapped hydrogen at various lattice defects such as dislocation and vacancy. It is reported that peaks of hydrogen desorption are dependence on thickness of specimen, heating rate, binding energy and defect density. Thus, the objective of the present study is the separation of the hydrogen states in pure iron emphasized dislocation and vacancy using controlling thickness of specimen and heating rate.