Evaluation of SCC Crack Growth Behavior of Non-Sensitized Stainless Steels in High Temperature Water by SSRT
-
- Kanzaki Manabu
- Sumitomo Metal Industries, Ltd.
-
- Takeda Kiyoko
- Sumitomo Metal Industries, Ltd.
-
- Kudo Takeo
- Sumitomo Metal Industries, Ltd.
Bibliographic Information
- Other Title
-
- SSRTによる非鋭敏化ステンレス鋼の高温水中SCCき裂進展挙動の評価
- SRTによる非鋭敏化ステンレス鋼の高温水中SCCき裂進展挙動の評価
- SRT ニ ヨル ヒエイビンカ ステンレスコウ ノ コウオン スイチュウ SCC キレツ シンテン キョドウ ノ ヒョウカ
Search this article
Description
Slow strain rate test (SSRT) method was applied to evaluate the SCC behavior of non-sensitized stainless steels in high temperature water. Crack growth rate (CGR) was evaluated by investigating the time dependence of the maximum crack depth in SSRT. The effects of materials and test conditions on the CGRs were studied. As the result, the CGR of non-sensitized 18Cr-8Ni stainless steels (SUS316, SUS304, SUS347) was in the range of (3−6)×10−10 m/s. In 316NG (nuclear grade), the CGR showed the highest at 561 K, and increased with the concentration of dissolved oxygen and conductivity. The CGR in SSRT was higher by 10 times than that obtained in the crack extension test using CT specimens.
Journal
-
- Corrosion Engineering
-
Corrosion Engineering 56 (6), 259-264, 2007
Japan Society of Corrosion Engineering
- Tweet
Keywords
Details 詳細情報について
-
- CRID
- 1390282681234776320
-
- NII Article ID
- 130004732238
-
- NII Book ID
- AN10235427
-
- ISSN
- 18819664
- 09170480
-
- NDL BIB ID
- 8862204
-
- Text Lang
- ja
-
- Data Source
-
- JaLC
- NDL Search
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed