For 6061-T6 and 7075-T6 aluminum alloys as candidate liner materials for high-pressure hydrogen container, SSRT (slow strain-rate technique) tests in humid air with 90% relative humidity were carried out to evaluate the susceptibility to hydrogen embrittlement (HE) and to reveal the process of HEAC (hydrogen-environment -assisted cracking). 7075-T6 showed a significant susceptibility to HE, resulting in intergranular cracking, while in contrast, 6061-T6 exhibited an excellent resistance required as liner materials. HEAC of 7075-T6 is confirmed to progress as follows; at the first stage micro-cracks originate at inclusions of Al–Fe–(Cu) phase on the specimen surface and then advance to intergranular cracking. 6061-T6 would not give rise to micro-cracks because of less localization of slip deformation enhanced by hydrogen effects, mainly due to the precipitation microstructure.
収録刊行物
-
- 軽金属
-
軽金属 56 (12), 721-727, 2006
一般社団法人 軽金属学会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390282681315352064
-
- NII論文ID
- 10018660937
-
- NII書誌ID
- AN00069773
-
- COI
- 1:CAS:528:DC%2BD2sXhvVWltLg%3D
-
- ISSN
- 18808018
- 04515994
-
- NDL書誌ID
- 8623525
-
- 本文言語コード
- ja
-
- データソース種別
-
- JaLC
- NDLサーチ
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可