T6 conditions were examined on the Al-6.85%Si-0.30%Mg-0.20%Fe-0.12%Ti-1.006%Na alloy castings to select an optimum heat treating condition for automobile wheels. Solution heat treating at 540°C for 9hr and quenching into cold water (15°C) as soon as possible are recommended. The elongation and Charpy impact value are reduced by quenching in hot water or quenching after prolonged delay time. Aging at 180°C for 6hr ensures the highest strength, and aging at 140°C for 4hr does high elongation and impact strength.
Journal
-
- Journal of Japan Institute of Light Metals
-
Journal of Japan Institute of Light Metals 28 (1), 8-14, 1978
The Japan Institute of Light Metals
- Tweet
Details 詳細情報について
-
- CRID
- 1390282681315654656
-
- NII Article ID
- 130004207956
- 10004011171
-
- NII Book ID
- AN00069773
-
- COI
- 1:CAS:528:DyaE1MXitVygtLg%3D
-
- ISSN
- 18808018
- 04515994
-
- NDL BIB ID
- 1923679
-
- Text Lang
- ja
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed