書誌事項
- タイトル別名
-
- Specific Heat Measurements on 10%Sn-Pb Alloy Aged at Various Temperatures. (On Precipitation of Tin from Lead-Tin Solid Solutions (4th Report))
- カクシュ オンド デ ジコウセル 10 Sn-Pb ゴウキン ノ ヒネツ ソクテイ
この論文をさがす
抄録
The aging process of 10%Sn-Pb alloy at 50°, 75°, 100° and 110° was studied by tracing the specific heat- versus-temperature curves. (1) At a temperature lower than about 112°, the precipitation of tin from lead takes place in two stages. At a higher temperature than about 112°, the precipitation of tin seems to be completed in one stage. (2) The kinetic law for the 2nd stage of the precipitation seems to be represented as follows; p=Ktn+C, where n is a constant independent of temperature and has the value of about 0.5. The activation energy for the 2nd stage was obtained from the relation between the rate constant K and the aging temperature T. The activation energy for the 2nd stage obtained in this investigation is ca. 18 kcal/mol and is in fair agreement with the earlier estimation of the activation energy for the 2nd stage obtained from the micro-hardness measurements, ca. 22 kcal/mol. These values of the activation energy for the 2nd stage are appreciably different from the activation energy for the 1st stage, ca. 9 kcal/mol.
収録刊行物
-
- 日本金属学会誌
-
日本金属学会誌 23 (3), 173-177, 1959
公益社団法人 日本金属学会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390282681458519296
-
- NII論文ID
- 130007333415
- 40018257388
-
- NII書誌ID
- AN00187860
-
- ISSN
- 18806880
- 24337501
- 00214876
-
- NDL書誌ID
- 9152828
-
- データソース種別
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可