- Extrusion Sintering of Harmonic-Structured Composite with Ti-48 mol%Al Alloy and Pure Titanium by SPS Process
- Ti-48 mol%Al/ジュンTi フクゴウ チョウワ ソシキ ザイリョウ ノ SPSホウ オ リヨウ シタ オシダシ ショウケツ
この論文をさがす
説明
A harmonic-structured composite with a fine grain Ti-48 mol%Al alloy network and dispersed coarse grain pure titanium is produced by extrusion sintering using the spark plasma sintering (SPS) process. The conditions of extrusion sintering by the SPS process are a sintering temperature of 1073 K, a holding time of 1.8 ks and an extrusion pressure of 100 MPa with a pressurization rate of approximately 0.1 MPa/s. The extrusion compact has a rod shape with φ5×48 mm. The extrusion compact is composed of an elongated harmonic structure with the Ti-48 mol%Al alloy network and the dispersed pure titanium. The Vickers hardness of the extrusion compact is about 220 Hv, which is almost the same as that of a conventional compact.<br>
収録刊行物
-
- 日本金属学会誌
-
日本金属学会誌 79 (7), 372-375, 2015
公益社団法人 日本金属学会
- Tweet
キーワード
詳細情報 詳細情報について
-
- CRID
- 1390282681459430016
-
- NII論文ID
- 130005084808
-
- NII書誌ID
- AN00062446
-
- ISSN
- 18806880
- 24337501
- 00214876
-
- NDL書誌ID
- 026603483
-
- 本文言語コード
- ja
-
- 資料種別
- journal article
-
- データソース種別
-
- JaLC
- NDLサーチ
- Crossref
- CiNii Articles
- KAKEN
- OpenAIRE
-
- 抄録ライセンスフラグ
- 使用不可