Magnetic properties of Fe-Pd-Ag alloys containing 17∼47 at%Pd and 1∼30 at%Ag have been measured. The coercive force of the alloys increases with increasing silver content to 12%. The 59 at%Fe, 29 at%Pd and 12 at%Ag alloy tempered after water-quenching has a coercive force of 95.5 kA·m−1, a residual magnetic flux density of 1.04T and a maximum energy product of 43.0 kJ·m−3. Another alloy containing 58 at%Fe, 32 at%Pd and 10 at%Ag wire-drawn has a higher coercive force of 115.4 kA·m−1, a residual magnetic flux density of 0.90T and a maximum energy product of 41 kJ·m−3.<BR>It is considered that the high coercivity of the alloy is due mainly to the high magneto-crystalline anisotropy of γ1 phase dispersed in α phase.

収録刊行物

  • 日本金属学会誌

    日本金属学会誌 45 (11), 1176-1179, 1981

    公益社団法人 日本金属学会

詳細情報 詳細情報について

問題の指摘

ページトップへ