<p>Phosphorus recovery from dehydrated waste water sludge by incineration using alkali metal compounds was carried out. The dehydrated sludge was mixed with NaOH, KOH or Na2CO3, and incinerated at 750 degree to 900 degree after drying treatment. Phosphorus was recovered by extraction using water. The phosphorus was recovered as a form of alkali metal phosphate, and recovery rate reached about 75%.</p>