SB-07-5(073) Development of 18Cr-9Ni-W-Nb-V-N Austenitic Stainless Steel Tube for Thermal Power Boilers(Changes in Microstructure 2) :
-
- ISHITSUKA,T.
- Nippon Steel Corporation, Steel Research Laboratories
-
- MIMURA,H.
- Nippon Steel Corporation, Pipe & Tube Sales Division
この論文をさがす
説明
An 18Cr-9Ni-W-Nb-V-N austenitic stainless steel tube for thermal power boilers has been newly developed. The high temperature mechanical properties and corrosion resistance of the steel were investigated. The creep rupture strength of the developed steel is about 1.5 times as high as that of SUS347HTB, and is almost the same as that of Ka-SUS310J2TB at 650℃. This excellent creep strength of the steel is mainly due to solid solution strengthening by tungsten and nitrogen, and precipitation strengthening by nitrides of niobium and vanadium. The carbon content of the steel is reduced to 0.03% to improve intergranular corrosion resistance. The steam oxidation resistance and the high temperature corrosion resistance of the tube are almost the same as those of SUS347HTB. Weldability of the developed steel is superior to that of SUS304HTB and SUS310TB. Thus the developed steel is suitable for use as a material for superheater and reheater tubes of thermal power boilers.
収録刊行物
-
- Creep : proceedings of the ... international conference on creep and fatigue at elevated temperatures
-
Creep : proceedings of the ... international conference on creep and fatigue at elevated temperatures 401-406, 2001-06-03
日本機械学会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1540854195276805504
-
- NII論文ID
- 110002494665
-
- NII書誌ID
- AA11901384
-
- 本文言語コード
- en
-
- データソース種別
-
- NDLデジコレ(旧NII-ELS)
- CiNii Articles