Physical Meaning of Wetting Curve Traced by Meniscograph Wettability Tester
-
- OKAMOTO I.
- Osaka University
-
- TAKEMOTO Tadashi
- Osaka University
-
- MIZUTANI Masami
- Osaka University
-
- MORI Ikuo
- Osaka University (Present office)TOSHIBA Ltd.
Search this article
Abstract
The wetting curve traced by a meniscograph wettability tester was analized physically by applying the equation of one-dimensional heat conduction. If the oxide film on a specimen is removed by surface preparation, the wetting curve of the specimen is the "locus of 456K (183℃)". Here, 456K is the melting point of a used solder. Therefore, the wetting rate or the wetting time are dependent only on the heat conductivity of the used specimen.
Journal
-
- Trans. JWRI
-
Trans. JWRI 14 (1), 21-27, 1985
Osaka University