Mechanical Properties of TiAl and (TiAl+Ti<sub>3</sub> Al) Alloys Produced by Mechanical Alloying

この論文をさがす

説明

<jats:title>ABSTRACT</jats:title><jats:p>Two representative titanium aluminides containing 48 and 52 at. pct Al were produced by a mechanical alloying (MA) process for the purpose of attaining fine microstructures. For the MA apparatus, an attritor mill and a conventional ball mill were both used and the results compared. Mechanically alloyed powders were consolidated by hot pressing. In addition to morphological changes in the powders during MA, microstructures and mechanical properties of the consolidated products were studied. In particular, the MA alloy with 48 at. pct Al comprised of both TiAl and Ti 33Al phases showed a high strain rate sensitivity exponent, above 0.3. This suggests a possibility of developing superplastic deformation.</jats:p>

収録刊行物

  • MRS Proceedings

    MRS Proceedings 196 1990-01-01

    Springer Science and Business Media LLC

詳細情報 詳細情報について

  • CRID
    1872272492806658176
  • DOI
    10.1557/proc-196-201
  • ISSN
    19464274
    02729172
  • データソース種別
    • OpenAIRE

問題の指摘

ページトップへ