Degradation of polyethylene by combination of thermal aging and radiation
説明
A 25 µm thick low density polyethylene film free from additives had been subjected to γ-irradiation with a dose rate of ca. 5.3×104 rad/hr at room temperature in air (denoted as γ) and/or thermal aging at 90 °C in air (denoted as HT). The order of oxidative degradation is (γ)≤(HT−γ)<(γ −HT)≃((γ,HT)), where () means the single or sequential application of γ and HT, the bar means the order of the application of them and ((γ,HT)) means the simultaneous application of γ and HT.
収録刊行物
-
- 1984 IEEE International Conference on Eletrical Insulation
-
1984 IEEE International Conference on Eletrical Insulation 271-274, 1984-06-01