An Investigation of the Deactivation Behavior of Industrial Mo/Al<sub>2</sub>O<sub>3</sub>and Ni-Mo/Al<sub>2</sub>O<sub>3</sub>Catalysts in Hydrotreating Kuwait Atmospheric Residue

この論文をさがす

説明

Abstract The catalyst system for fixed-bed residue hydrotreating processes usually consists of different types of catalysts designed to promote hydrodemetallation (HDM), hydrodesulfurization (HDS) and hydrodenitrogenation (HDN) reactions to desired levels. Overall catalyst life is determined by the performance of the individual catalysts in the different reactors. Therefore, information about the activity, stability, selectivity, and deactivation behavior of the individual catalyst is highly desirable to design improved catalysts that can prolong catalyst life, increase stream efficiency, and improve process economics. In the present work, residue hydrotreating experiments were conducted on two types of industrial hydrotreating catalysts, namely Mo/Al2O3 and Ni-Mo/Al2O3, that have been used as HDM and HDS catalysts, respectively, in an industrial ARDS process. The primary objective of the study was to compare the deactivation behavior of both types of catalyst. The characterization of the used catalysts b...

収録刊行物

詳細情報 詳細情報について

  • CRID
    1874242817673583360
  • DOI
    10.1081/lft-200030942
  • ISSN
    15322459
    10916466
  • データソース種別
    • OpenAIRE

問題の指摘

ページトップへ