シラスの工業的利用に関する研究 (第8報) : シラスを原料とする白色タイル素地

書誌事項

タイトル別名
  • Studies on the industrial application of "SHIRASU" (Report 8) : on the preparation of lightweight tile using "SHIRASU"
  • シラスの工業的利用に関する研究-8-シラスを原料とする白色タイル素地
  • シラス ノ コウギョウテキ リヨウ ニ カンスル ケンキュウ 8 シラス オ ゲンリョウ ト スル ハクショク タイル キジ

この論文をさがす

抄録

A little amount of white cement, kaolin and wollastnite is added to magnetic separated and selected SHIRASU, the mixture then press moulded and fired in the electric furnace. Physical and thermal Properties and bending strength of those fired bodies were investigated. The properties of SHIRASU-white cement-kaolin system or SHIRASU-white cement-wollastnite system fired at 1150 to 1200°C are as follows, apparent gravity 2.3~2.7, bulk gravity 1.8~2.0, water absorption 0~17(%), bending strength 80~500kg/cm^2, and thermal expansion coefficient is found in the following region "5.6~5.8×10^{-6}". The whiteness of the tile bodies SHIRASU is 90(%), near the pure white, so that colouring is good and can be expected the reduction of pigment consumption.

収録刊行物

詳細情報 詳細情報について

問題の指摘

ページトップへ