2ヒドロキシエチルメタクリレート(HEMA)ポリマーおよびHEMA加工絹糸の構造特性
-
- 塚田 益裕
- 農林水産省蚕糸試験場
書誌事項
- タイトル別名
-
- Structural characteristics of 2-Hydroxyethyl Methacrylate (HEMA)-grafted silk.
- 2 ヒドロキシエチルメタクリレート HEMA ポリマー オヨビ HEMA カコ
この論文をさがす
説明
Structural characteristics of HEMA polymer and HEMA-grafted silk were studied by means of differential scanning calorimetry (DSC), x-ray diffraction and scanning electron microscopy (SEM).<br>Keton type carbonyl radicals were formed in associating with the dehydration of the intermolecular side chains of HEMA polymer, when the temperature exceeded 200°C. Melting was accompanied bythe degradation of the molecular chains of HEMA polymer at about 314°C. The temperature of thermal decomposition of the HEMA-grafted silk shifted to higher values with the increase in the graft percentage of HEMA polymer. The decomposition temperature of HEMA-grafted silk containing more than 90% HEMA polymer reached 340°C. The enthalpic change of the endothermic peak which appeared at 410°C on the DSC curves of HEAM-grafted silk remained unchanged even after the increase in the graft percentage of HEAM polymer.<br>Crystalline structure and adsorptive behavior of the HEMA-grafted silk remained unchanged even after HEMA grafting. Scaning electron micrographs of the HEMA-grafted silk containing more than 90% HEMA polymer showed granular forms on the surface of the HEMA-grafted silk.
収録刊行物
-
- 日本蚕糸学雑誌
-
日本蚕糸学雑誌 53 (5), 380-386, 1984
社団法人 日本蚕糸学会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390001204529542016
-
- NII論文ID
- 130003834358
-
- NII書誌ID
- AN00190300
-
- ISSN
- 1884796X
- 00372455
-
- NDL書誌ID
- 3008409
-
- 本文言語コード
- ja
-
- 資料種別
- journal article
-
- データソース種別
-
- JaLC
- IRDB
- NDLサーチ
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可