The kinetics of reoxidation of Al killed steel with slag and air were investigated in laboratory experiments using tammann furnace and in plant experiments using commercial 85×103 kg tundish. Experimental results were discussed by the coupled reaction model.<BR>Observed apparent rate constants of [sol.Al] decreased with increasing (CaO)/(SiO2) ratio in laboratory experiments and showed a good agreement with calculated ones.<BR>Flow rate of air leak at steady state was evaluated to be 3.0×10-5 and 4.0×10-4 m3/s inside and outside of immersion tube in commercial tundish, respectively and was estimated to have little influence on reoxidation.<BR>Mass transfer coefficient in metal was estimated to be 6.0×10-5 m/s based on the tundish mixing model and the coupled reaction model.<BR>Observed [sol.Al] in tundish decreased with increasing (%FeO)+(%MnO) value in ladle slag and showed a good agreement with calculated one by considering reoxidation in ladle and air leak at unsteady state.

収録刊行物

  • 鉄と鋼

    鉄と鋼 85 (5), 375-381, 1999

    一般社団法人 日本鉄鋼協会

被引用文献 (4)*注記

もっと見る

参考文献 (27)*注記

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ