Effect of Impurity Ions and Additives in Solution of Copper Electrorefining on the Passivation Behavior of Low-Grade Copper Anode
-
- Mori Kohei
- Department of Materials Process Engineering, Graduate School of Engineering, Kyushu University
-
- Yamakawa Yuta
- Department of Materials Process Engineering, Graduate School of Engineering, Kyushu University
-
- Oue Satoshi
- Department of Materials Science & Engineering, Faculty of Engineering, Kyushu University
-
- Taninouchi Yu-ki
- Department of Materials Science & Engineering, Faculty of Engineering, Kyushu University
-
- Nakano Hiroaki
- Department of Materials Science & Engineering, Faculty of Engineering, Kyushu University
Bibliographic Information
- Other Title
-
- 低品位銅アノードの不動態化挙動に及ぼす銅電解精製浴中の不純物イオンと添加剤の影響
Search this article
Description
<p>The Cu electrorefining using low-grade copper anode is desired from the view point of reduction of electric power. Cu electrolysis was performed using a low-grade copper anode in an unagitated sulfate solution, and the effect of impurity ions and additives in solution on the passivation of anode was investigated. The time when anode passivation firstly occurs shortened significantly in solution containing 0.596 mol·dm−3 of Ni2+ ions as impurity, and shortened somewhat in solution containing As5+(0.053 mol·dm−3) or Bi3+(0.0005 mol·dm−3) ions. Sn2+(0.0004 mol·dm−3) and As3+(0.053 mol·dm−3) ions slightly decreased the time to passivation, but Sb3+ (0.004 mol·dm−3) ions rarely decreased the time. When the 0.596 mol·dm−3 of Ni2+ ions were added in solution, the viscosity coefficient of solution increased and the diffusion coefficient of Cu2+ ions decreased. When the As5+(0.053 mol·dm−3) or Bi3+(0.0005 mol·dm−3) ions were added in solution, the compound of As-Sb-O or As-Bi-O system was formed in anode slime, which seemed to increase the compactness of slime. The time to passivation was slightly longer in thiourea-free solution, but shortened with increasing the concentration of thiourea from 0.525 to 2.24 mmol·dm−3. In the solutions containing 0 to 1.13 mmol·dm−3 of Cl− ions, the time to passivation was constant, but significantly shortened with increasing the concentration of Cl− ions at the region above 1.13 mmol·dm−3. Cl− ions formed CuCl at the upper area of anode slime, as a result, increased the compactness of slime and promoted the passivation.</p>
Journal
-
- Journal of the Japan Institute of Metals and Materials
-
Journal of the Japan Institute of Metals and Materials 86 (6), 97-106, 2022-06-01
The Japan Institute of Metals and Materials
- Tweet
Keywords
Details 詳細情報について
-
- CRID
- 1390010765214032128
-
- NII Book ID
- AA1151294X
-
- ISSN
- 18806880
- 24337501
- 13475320
- 00214876
- 13459678
-
- HANDLE
- 2324/7172648
-
- NDL BIB ID
- 032589584
-
- Text Lang
- ja
-
- Data Source
-
- JaLC
- IRDB
- NDL Search
- Crossref
- KAKEN
- OpenAIRE
-
- Abstract License Flag
- Disallowed